film
Industrial film
NDT film (N0n-Destructive Testing film)
Our industrial film use Japanese FUJI importing big roll films to cut and pack. This films can use X-ray or gamma ray to NDT for object.
They have high photonasty, high contrast, very sophisticated veins and high clear degree, is very good NDT films.
They have super thin particle size, can easy to check workpiece defect. Photosensitive coating is very equality. The different batch products have kind stability. So batch products needn't adjust usually exposal condition, and get steady & density homogeneous image.
1) IXQ100 film = D7, fit automatic develop film
2) IXQ80 film=D4, it's gamma film
3) IXQ100HD= Kodak AA400, fit manual develop film
8cm x30cm x100
8cm x36cm x100
12'x15'x100
14'x17'x100
7cmx305cm x1
8cm x305cm x1
Specification and Packaging
Specification |
Package |
British system
(inch) |
metric system
(mm) |
packaging of box
(pcs) |
Quantity of per Carton(box) |
Weight(kg) |
Size of Carton
(mm) |
80×180 |
100 |
10 |
10 |
358×240×250 |
80×240 |
100 |
10 |
10 |
358×240×250 |
80×300 |
100 |
10 |
10 |
358×240×250 |
80×360 |
100 |
10 |
13 |
415×240×250 |
12×15 |
305×381 |
50 |
5 |
16 |
438×203×365 |
14×17 |
356×432 |
50 |
5 |
21 |
490×203×415 |
14×17 |
356×432 |
100 |
4 |
32 |
500×243×435 |
80×6000 |
1 roll |
6 |
13 |
440×310×250 |
|
Flushing Process Conditions |
Developing and fixing recommended formula and technology: |
Reference formulas |
Temperature |
time |
Developing |
our developing solution |
20°C |
4~6 mins |
fixing |
our fixing solution |
20°C |
10 mins |
watering |
room temperature |
15 mins |
|
|
Remark
1.The products should be stored in a cool and dry place. It should be avoided the exposure to harmful gas and avoided the damage by pressure.
2.Sealed box should store in a cool (50 to 70 degrees Fahrenheit to Celsius, relative humidity
30-50%), and preventing the effects from other x-ray.
3.Please use up timely after unpacking, avoiding damp and stick.
4.12 months guarantee |
All kinds of size, welcome to choice.